An aluminium reduction cell runs at 940–970 °C and turns roughly half of its electrical input into waste heat. Where that heat leaves is not a detail. Published heat balances put 35–40 % of the loss through the sidewall and only 5–15 % through the bottom; the sidewall figure is deliberate, because a frozen bath ledge has to be maintained there, while the bottom is insulated to keep the cathode clean. Two opposite thermal requirements sit inside one steel shell. Our application map places SLM-1000/1200 microporous insulation board behind dense refractory as a cold-face backup layer; in a cell that means the sub-cathode build-up, and emphatically not the sidewall. This is a product guide: what the board is, what its conductivity means at 200–800 °C, how to pick grade, facing and thickness from the isotherm the designer must hold, where it sits under the cathode, how to cut, fix and seal it, and where it is the wrong material. One limitation up front: no independent or peer-reviewed field measurement of microporous board in a reduction cell was found. Cell data below sets the selection inputs; it is not a measured saving.
What the product is, and what it is not
The board is a pressed composite of fumed silica, reinforcing fibre and an opacifier. Pores smaller than the mean free path of air suppress gas conduction and convection together, while the opacifier scatters the infrared radiation that dominates above 400 °C. How the board is manufactured explains the difference from a fibre blanket: no fibrous network to compress, no organic binder to burn out, no open cell for bath vapour to circulate through. Commercial grades span 1000, 1100 and 1200 °C classification temperatures, densities near 230–400 kg/m³, compressive strengths of 0.12–0.94 MPa, and thicknesses from 3 to 50 mm. Facings include E-glass cloth, PE film, aluminium foil, mica laminate and hydrophobic cores. Panels can be cut, sawn, drilled, punched or CNC-cut to a relining drawing. A1 non-combustibility is a material property, not a fire-protection rating.
One number is routinely misread. Classification temperature is a short shrinkage test — Promat defines it as less than 2 % linear shrinkage after a 24-hour full soak under ASTM C356 — not a continuous working limit. A Morgan datasheet records 3.8 % shrinkage after 24 hours at its own 1000 °C classification temperature, against 0.6 % for a 12-hour single-face soak. Shrinkage is meaningless without the soak condition; a 1000-grade product is quoted at 950 °C continuous in one catalogue. Ask which definition is on the certificate.
The product boundary follows. This is a cold-face backup insulator, not a working lining, not a penetration barrier, not a structural layer and not a fire-protection device. Water, oil and petroleum spirits irreversibly destroy the microporous structure, in the words of a SILCA datasheet, so facing, edge sealing and packaging are part of the specification.
Product conductivity at cathode-backup temperatures
Published curves for the SLM grades give about 0.020 W/m·K at 20 °C, 0.022 at 200 °C, 0.025 at 400 °C and 0.033 at 800 °C. Independent commercial datasheets sit in the same band: MICROTHERM PANEL-1000R lists 0.023 / 0.026 / 0.031 / 0.039 W/m·K at 200 / 400 / 600 / 800 °C, Morgan WDS Ultra Board 0.022 / 0.027 / 0.034 / 0.044, and a 1200-grade panel 0.029 / 0.033 / 0.039 / 0.044. The datasheet guide explains how to read these as mean-temperature values tied to a test method and a density before using them in a calculation. | Mean temperature | Microporous board | Ceramic-fibre blanket | Calcium silicate | |---|---|---|---| | 200 °C | 0.022–0.023 W/m·K | ~0.06 W/m·K | ~0.055 W/m·K | | 400 °C | 0.025–0.027 W/m·K | ~0.10–0.12 W/m·K | ~0.10 W/m·K | | 600 °C | ~0.029–0.034 W/m·K | ~0.15–0.17 W/m·K | ~0.12 W/m·K | | 800 °C | 0.033–0.044 W/m·K | ~0.22–0.27 W/m·K | ~0.14 W/m·K |
Insulating firebrick is quoted near 0.125–0.160 W/m·K over 200–600 °C. These comparison values come from supplier data pages, not one comparative test programme; confirm them against the relining bill. The board's curve is nearly flat while fibrous and calcium-silicate alternatives steepen, which lets a backup layer be thin. Above about 600 °C radiation through the pores becomes significant, and one patent argues for graded layers rather than a single sheet at the hottest position — a design argument, not a measured failure.
Selecting grade, facing and thickness from the 850 °C isotherm
A 960 °C bath does not expose a bottom panel to 960 °C. What the panel sees is the cold face of the dry anti-seepage or barrier layer in front of it. Published cell designs add a harder constraint: the 850 °C penetration isotherm must sit inside the refractory or barrier bricks, not in the insulation, and the space below the cathode blocks is only about 250–350 mm. Salt reaching that far would raise the insulation's conductivity and push the isotherm further down.
Grade is chosen from the worst case at that interface, not from the bath temperature. The SLM-1000 and SLM-1200 comparison sets out where the higher grade pays; in a cell the excursion case matters more than the average, because an anode effect can push electrolyte temperature above 1000 °C briefly and a thinned barrier raises the interface everywhere beneath it. Ask for shrinkage data at that temperature with the soak condition stated. Facing is the second decision. Aluminium foil gives a clean skin and a vapour barrier; hydrophobic grades suit positions where condensation during a shutdown is plausible; PE film is a dry-handling option. Datasheets note that facings also protect the core from water in mortars and castables. Every cut edge is sealed the day it is cut.
Thickness follows from the allowable bottom heat flux, and the thickness-sizing method guide gives the full calculation. An illustrative example: assume a 350 °C barrier cold face, an 80 °C steel floor target and 300 W/m² allowed by the cell designer. Required resistance is (350 − 80) / 300 ≈ 0.90 m²·K/W. At a mean board conductivity near 0.027 W/m·K that is about 33 mm of board, against roughly 90 mm of calcium silicate at 0.10 or 120 mm of fibre blanket at 0.13. Those inputs are design assumptions, not measured cell values; no public bottom heat-flux limit for this cell type was found. In a cell the useful output is often not total lining thickness but what remains of the fixed sub-cathode space. A thinner backup leaves more of the 250–350 mm for barrier brick and dry anti-seepage material, which is where the 850 °C isotherm is supposed to stay. That is a geometry argument to check against the cell designer's thermal model, not a licence to move the isotherm.
Where the board goes: the sub-cathode build-up
Published lining sections describe, from the outside in, a steel bottom plate around 8–12 mm, calcium silicate board roughly 50–65 mm, two courses of lightweight insulating brick near 65 mm each, a dry anti-seepage layer around 130–195 mm, and cathode carbon blocks near 450 mm. Bath at 940–970 °C sits above, with a metal pad and electrolyte each around 200 mm in one dissertation. Sidewalls use a different build-up, often Si₃N₄-bonded SiC bricks against the ledge.
Read as a product rule: the board is a candidate only for the backup portion of the bottom build-up, behind the barrier layer. It replaces part of the calcium silicate or insulating brick thickness. It does not replace the dry anti-seepage layer, whose job is to stop bath and sodium reaching the insulation, and it does not go into the cathode block or the sidewall.
This is the same cold-face discipline used in aluminium holding furnaces, where the board sits behind the refractory that sees molten metal, and in carbon anode baking furnaces, where it belongs in covers and casing backup rather than in load-bearing flue walls. All three positions share one rule: a dense, chemically resistant layer faces the process, and the board works on the cold side of it. Why the board must not go on the sidewall
The frozen ledge is mostly cryolite with a little CaF₂, and its thickness is a function of the heat flow through the sidewall. That is why 35–40 % of the cell's heat loss is designed to leave through the sides. It is not waste to be recovered with more insulation; it is the mechanism that keeps a protective solid layer between the corrosive bath and the lining.
Published cell studies and patents describe both failure directions. A sidewall with high thermal resistivity will not maintain the ledge, leaving refractory exposed to chemical attack and, in extreme cases, a red-hot shell and tap-out; one patent calls overinsulation a cause of deeper fluoride-salt penetration and shorter cell life. An over-cooled side builds a thick ledge, disturbs current distribution, encourages sludge and can trigger anode effects. Ledge thickness must be modelled against cell current and superheat; a teaching model balances 10 K at about 12.6 cm of ledge, but that is an illustration, not a measurement.
So the board is not a candidate for the sidewall or the ledge zone. Any proposal to line the shell sides must be checked against the ledge profile, the current density and the shell heat-flow target by the cell designer. A falling side-shell temperature is not automatically a win. Cell-lining models note that the lining does not conduct current; magnetic effects act on the metal and bath, with only indirect coupling through the ledge shape.
The published record needs a warning here. A Chinese trade-press report describes a six-cell trial with a 10 mm nano-porous layer on the inner shell wall, claiming 20–24 °C lower side-shell temperature, 5–8 °C at the bottom, 40–60 mV lower voltage and 91.3 % current efficiency. It gives no cell type, measurement protocol, ledge profile or third-party verification; it is a plant self-report reproduced by industry media, not an independent measurement. A side-shell drop of that size is exactly what must be reconciled with ledge stability before being called a benefit.
What a relining cycle does to the board specification
A cell lining is a long-service, one-shot installation. Published pot life figures run from about 1500 to 3000 days, with a mean near 2000 days in one TMS study; relining is quoted at roughly 2.1 % of production cost and US$50,000–300,000 per pot, and even a controlled shutdown can permanently cost 100–400 days of cathode life. The insulation installed at a relining has to survive that whole interval, because there is no cheap mid-life access to it.
That changes what to ask for. A single heat-up and years at steady temperature impose fewer cycles than a cyclic furnace, but the consequence of creep, settlement or salt penetration is far larger. Specify shrinkage with its soak condition, tolerances tight enough that panels cannot settle into gaps, and a facing that will not debond over years. Enhanced-strength or mica-laminated grades exist where clamping loads are higher.
It also changes the buying sequence. Panels are cut to a relining drawing, matched to cathode block modules and delivered into a narrow shutdown window; a missing size or a damaged moisture barrier delays a pot that costs money every day it is down. Cut list, packaging and delivery date are part of the product specification, not logistics detail.
Why the board stays behind the penetration barrier
Chemistry is the first reason. Peer-reviewed work on aluminosilicate lining materials shows cryolitic bath attacking them above about 700 °C, with molten NaF and metallic sodium as the main agents; EPMA work identifies sodium vapour as the reaction front, producing nepheline, albite and sodium aluminate. A 2025 ICSOBA review gives the strongly exothermic reaction between liquid aluminium and SiO₂. Those studies concern refractory bricks and barrier materials, not microporous board, and no dedicated compatibility study between fumed-silica board and cell bath was found. The design inference is nevertheless clear: a silica-rich panel must sit behind a gas-tight barrier, never in a position where bath, metal or sodium vapour can reach it.
The isotherm is the second reason. If the 850 °C line migrates into the insulation, penetrating salts raise its conductivity and accelerate the same migration. Keeping the barrier layer thick enough is a thermal design task; adding board behind it does not repair a failed barrier.
Mechanics is the third. At 0.12–0.94 MPa compressive strength the board cannot carry cathode blocks, collector bars, a worker or the cradle. Steel-shell distortion and sodium-expansion stresses belong to the shell's structural design. Moisture is the fourth: a wet panel inside a sealed cathode is unreachable, and the pore damage is permanent.
Cutting and installing the board: joints, fixing and moisture
Panels are cut to the relining drawing with standard tools, which helps around collector-bar openings and end-wall returns. Two failure modes come with that convenience. The first is the open joint: a narrow gap through a 33 mm panel bypasses the pore structure and behaves as a thermal bridge. Fit panels tight, stagger joints, pack residual seams with compatible fibre and allow 1–2 mm for expansion at steel interfaces. The joint-gap control notes give the tolerances and packing detail; collector-bar penetrations and shell corners are where this fails. The second is moisture. Panels arrive in sealed moisture-barrier packaging, are stored flat and dry off the floor, and are cut only when ready to fit. Storage and cutting guidance covers the handling sequence. Wetted panels are rejected, not dried and reused. Pin holes should be 1–2 mm oversize for thermal expansion, and foil faces lapped and taped; a panel clamped rigidly against a shell that moves will crack. Fixing needs its own check. Glue, anchors, pins and clips are all listed in datasheets, but a fastener that bridges from the cold shell into the barrier zone becomes a heat path and a corrosion site. Where the shell detail cannot be adapted, retain panels with a light frame on the cold side rather than penetrating the barrier layer. Never use the board to close an expansion gap that was designed to move.
Incoming inspection and board acceptance
The incoming QC checklist covers dimensional tolerance, thickness uniformity, density, facing integrity, edge sealing, package moisture indication and certificates against the order. For a cell add three items: the shrinkage figure with its soak condition, written confirmation of the continuous service temperature, and the calculated 850 °C isotherm position in the agreed build-up. The meaningful check is a shell-temperature and heat-flux survey at defined points on the bottom and sides, logged with cell current, bath temperature, superheat, ambient conditions and pot age. Performance verification guidance describes the instrumented approach; a reading from a different pot is not comparable. Side-shell temperature trends are already used as a lining-condition and life-ranking signal, so side and bottom readings belong in the same baseline rather than being optimised separately. A local hot area usually means a gap, a displaced panel, a failed edge seal or a crack in the barrier in front of it — the failure analysis notes show what moisture and crushing do to this material — and rarely insufficient thickness. Record the survey as the baseline for later trending, and keep the ledge profile in the acceptance record. Where the board is not the answer
The sidewall and the ledge zone. Sidewall heat loss is what maintains the frozen ledge. Overinsulating it risks ledge melt-back, exposed refractory, chemical attack and tap-out. This is a thermal-design decision, not a product upgrade.
The hot face and the working lining. A 940–970 °C bath with dissolved alumina, metal and cryolite is outside the board's rating and chemical capability. Cathode carbon, SiC side bricks and barrier materials do that job.
The penetration barrier. Dry anti-seepage material stops bath and sodium before they reach the insulation. A porous panel cannot substitute for it, and no compatibility study supports that position.
Anywhere the 850 °C isotherm can reach. Penetrating salts raise conductivity and push the isotherm further down. A thinner backup must leave enough room for the barrier, not consume it.
Load-bearing and clamped positions. At under 1 MPa compressive strength the board cannot carry cathode blocks, collector bars, cradle loads or maintenance traffic.
Positions that can get wet. Wash water, a leaking service line or shutdown condensation destroys the pore structure permanently, and a cathode is not accessible for replacement.
Excursions above the continuous rating. Anode effects and a thinned barrier raise the interface. Selecting from the average bath temperature invites shrinkage and opened joints.
Cell operating problems. Ledge instability, anode effects, cathode voltage drop, bath chemistry and shell distortion are cell-design and operating issues. A thinner backup changes bottom heat loss; it does not fix them.
Buying the board: RFQ inputs and packaging
Specify grade, thickness, facing, panel dimensions and cut list together, and call out sealed moisture-barrier packaging, edge-sealing material and the shrinkage test condition. Ask for the current datasheet with its conductivity curve and written confirmation of the continuous service temperature at the design interface. High-strength nano insulation boards are listed on the SLM product page; use that as the quotation reference so conductivity is compared at the same mean temperature and density. A workable RFQ states cell type and technology supplier, current in kA, pot age, the full cathode lining section with every layer thickness, cathode block and collector-bar design, bath temperature, superheat and chemistry, target ledge profile, measured side-shell and bottom temperatures, hot spots, the relining window and allowable shell heat flux. Without the ledge and heat-balance inputs, a sidewall recommendation is unsafe and a bottom one is a guess.
Panels ship flat on pallets and are brittle and moisture-sensitive, so packaging and the delivery date are part of the price comparison. Container loading notes cover palletising, weather protection and keeping panels dry through an overseas project and site lay-down. Frequently asked questions
Can the board be applied to the sidewall as well as the bottom? No, not as a routine upgrade. Sidewall heat flow maintains the frozen ledge; changing it requires a cell thermal model and a ledge check by the designer.
How is thickness chosen? From the barrier cold-face temperature, the allowable bottom heat flux and the position of the 850 °C isotherm. The worked example gives about 33 mm for a 0.90 m²·K/W requirement, with inputs stated as design assumptions.
Are there published energy or shell-temperature results? No independent or peer-reviewed field measurement of microporous board in a reduction cell was found. The figures circulating in trade press are plant self-reports without a stated measurement protocol.
What facing is recommended? Foil-faced or hydrophobic grades with all cut edges sealed, because the cathode is sealed for years and cannot be inspected. PE film is a dry-handling option.
How is a failing installation detected? By a shell-temperature and heat-flux survey at defined points, trended against cell current, bath temperature and pot age. A new hot spot usually means a joint, a fixing or a crack in the barrier in front of the panel.
Bottom line
Microporous insulation board earns its place in a reduction cell by providing large thermal resistance in small thickness at the one position where extra resistance is wanted: the cold side of the bottom barrier, inside a fixed sub-cathode space. It can free thickness for the anti-seepage layer that holds the 850 °C isotherm. It does not face the bath, carry the cathode, replace the barrier, tolerate water or belong on a sidewall whose heat loss is keeping the ledge frozen. Specify it from the worst-case interface temperature and the cell's heat balance, keep it behind a gas-tight barrier, control joints and moisture, and verify with a like-for-like shell survey that includes the sides. Where chemistry, temperature, load or ledge stability can reach the board, choose a different material.
Data levels: bath temperature, bath chemistry, anode-effect behaviour, heat-loss split, specific energy consumption, lining build-ups, the 850 °C penetration isotherm, ledge behaviour, pot life and relining costs from peer-reviewed papers, ICSOBA/TMS conference papers, dissertations and patent literature; conductivity, density, strength, classification temperature definitions, shrinkage conditions, facings and liquid sensitivity from commercial microporous insulation datasheets, with SLM values from our own current datasheet; the trial figures quoted in the sidewall section from a plant self-report reproduced in trade press, not an independent measurement. Comparison conductivity values for fibre, calcium silicate and insulating brick come from supplier data pages. The resistance calculation is a one-dimensional steady-state estimate with its assumptions stated. No public instrumented measurement of a microporous-board retrofit on a reduction cell was found, and no dedicated study of fumed-silica board compatibility with cryolitic bath was found. Confirm all product values against the current SLM datasheet before specification.